TP008 – The Effect of Phase Compositions on the Pitting Corrosion of 25Cr Super Duplex Stainless Steel in Chloride Solutions

TP008 – The Effect of Phase Compositions on the Pitting Corrosion of 25Cr Super Duplex Stainless Steel in Chloride Solutions

Description:

This paper summarises part of the development process of Ferralium® 255. By carefully controlling of solution annealing process it is possible to optimise the combination of ferritic and austenitic phases present, thereby enhancing the corrosion resistance.

 